Lapaʻa Basalt
ʻO nā lālā basalt he mau fiber mau i hanaʻia e ke kaha kiʻekiʻe o ka platinum-rhodium alloy wire-drawing leak plate ma hope o ka hoʻoheheʻeʻiaʻana o ka mea basalt ma 1450 ~ 1500 C. E like me ke aniani fibers, aia kona mau waiwai ma waena o ka ikaika kiʻekiʻe o ka S aniani fibers a me ka alkali-free E aniani fibers. He ʻeleʻele maʻamau ka waihoʻoluʻu basalt maoli, a he gula kekahi.
Hiʻona Huahana
●Ka ikaika tensile kiʻekiʻe
●Ke kū'ē i ka corrosion maikaʻi
● Haʻahaʻa haʻahaʻa
● ʻAʻohe conductivity
●Pahana-pale
●Non-magnetic, uila insulation,
●Ka ikaika kiʻekiʻe, ka modulus elastic kiʻekiʻe,
● ʻO ke koena hoʻonui wela e like me ke kaʻa.
● Kū'ē kiʻekiʻe i ka corrosion kemika, acid, alkali, paʻakai.
Palapala noi
1. He mea kūpono no ka resin thermoplastic i hoʻoikaika ʻia, he mea kiʻekiʻe ia no ka hana ʻana i nā plastic molding sheets (SMC), block molding plastics (BMC) a me ka lump molding plastics (DMC).
2. Hoʻohana ʻia i mea hoʻoikaika ʻia no ke kaʻa, kaʻaahi a me ka pūpū moku.
3. E hoʻoikaika i ka sima a me ka asphalt, nā hiʻohiʻona anti-seepage, anti-cracking and anti-compression, E hoʻolōʻihi i ke ola lawelawe no Hydroelectric dam.
4. E hooikaika i ka paipu sima mahu no ka halekiai hooluolu a me ka mana nukili.
5. Hoʻohana ʻia no ke kiʻekiʻe wela o ka needling manaʻo: kaʻa kaʻa kani hoʻoheheʻe pepa, wela ʻōwili kila, alumini paipu, etc.
Papa inoa Huahana
Monofilament anawaena he 9 ~ 25μm, paipai 13 ~ 17μm; ʻO ka lōʻihi o ka ʻokiʻoki he 3 ~ 100mm.
Manaʻo:
Loihi(mm) | ʻAno wai(%) | Ka nui o ka maʻiʻo(%) | Ka nui a me ka noi |
3 | ≤0.1 | ≤1.10 | No nā pale kaʻa a me ka uhi no ka thermoplasticNo ka NylonNo ka hoʻoikaika ʻana i ka lāʻau no ka hoʻoikaika ʻana i ka asphalt No ka hoʻoikaika sima No nā mea hoʻohuihui No ka moena ʻaʻole i ulana ʻia, ka pale. Hoʻohui ʻia me nā fiber ʻē aʻe |
6 | ≤0.10 | ≤1.10 | |
12 | ≤0.10 | ≤1.10 | |
18 | ≤0.10 | ≤0.10 | |
24 | ≤0.10 | ≤1.10 | |
30 | ≤0.10 | ≤1.10 | |
50 | ≤0.10 | ≤1.10 | |
63 | ≤0.10-8.00 | ≤1.10 | |
90 | ≤0.10 | ≤1.10 |